Activation volume of various alloys at 25°C.
MetalStrain rate (s−1)True strainActivation volume (ν*/b3)Reference
316L stainless steel1000–30000.11.3current study
6000 series Al-Sc alloy1200–32000.14.2[28]
Unweldable Al-Sc alloy1200–32000.11.9[26]
Weldable Al-Sc alloy1300–32000.12.4[27]
Biomedical Ti alloy800–30000.11.11[25]