Home
|
Overview
|
Journals
|
Submit Manuscript
|
Contact Us
|
Français
Enter Your Search:
Search tips
Search criteria
Articles
Journal titles
Advanced
|
Bioinorg Chem Appl
|
v.2011; 2011
From:
Bioinorg Chem Appl.
2011;
2011
: 173782.
Published online 2011 December 20.
doi: 10.1155/2011/173782
Copyright/License
Request permission to reuse
Copyright
© 2011 Woei-Shyan Lee et al.
This is an open access article distributed under the Creative Commons Attribution License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.
Table 2
Work-hardening rate of various alloys at 25°C.
Metal
Strain rate (s
−1
)
True strain
Work-hardening rate (MPa/unit strain)
Reference
316L stainless steel
1000
0.1
1500
current study
6000 series Al-Sc alloy
1200
0.1
403.2
[
28
]
Unweldable Al-Sc alloy
1200
0.1
200
[
26
]
Weldable Al-Sc alloy
1300
0.1
160
[
27
]
Biomedical Ti alloy
800
0.1
250
[
25
]